| PROPERTIES |
ASTM TEST
METHOD |
HOMOPOLYMER
POLYPROPYLENE |
COPOLYMER
POLYPROPYLENE |
| Resistencia a la tensión-PSI |
D 638 |
4,800 |
4,000 |
| Tensile Elongation al Yield % |
D 638 |
12% |
23% |
| IZOD Impact Notched Ft lb/in @ 73°F |
D 256 |
1.9 |
7.5 |
| Heat Deflection Temp. °F @ 66 PSI |
D 648 |
210 |
173 |
| Mean Coefficient of Linear Thermal Expansion In/in °F |
D 696 |
6.2 X 10-5 |
6.6 X 10-5 |
| Maximum Operating Temperature °F |
Poly HI Solidur recommends |
180 |
170 |