PROPERTIES |
ASTM TEST
METHOD |
CHLORINATED
POLYVINYL CHLORIDE (CPVC) |
POLYVINYL
CHLORIDE (PVC) |
POLYVINYLINDENE FLUORIDE
(PVDF) |
Tensile Strength Yield-PSI |
D 638 |
8,200 |
N.A. |
6,300 |
Tensile Elongation al Yield % |
D 638 |
27% yield & break |
N.A. |
10% |
IZOD Impact Notched Ft lb/in @ 73°F |
D 256 |
1.6 |
0.8 |
3.5 |
Heat Deflection Temp. -I !F @ 66 PSI |
D 648 |
230 |
167 |
240 |
Mean Coefficient of Linear Thermal Expansion In/in °F |
D 696 |
3.7 X 10-5 |
6.1 X 10-5 |
6.2 X 10-5 |
Maximum Operating Temperature °F |
Poly HI Solidur recommends |
200 |
140 |
300 |